Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.945 g/cc @Temperature 37.8 °C |
0.0341 lb/in³ @Temperature 100 °F |
|
Paratherm Corporation Paratherm™ HR™ Heat Transfer Fluid Paratherm HR™ Heat Transfer Fluid is an alkylated-aromatic based heat transfer fluid formulated for closed loop liquid phase heating to 650°F in fired heaters and 675°F in waste heat recovery and.. |
|||
Density | 0.943 - 0.951 g/cc @Temperature 23.0 °C |
0.0341 - 0.0344 lb/in³ @Temperature 73.4 °F |
|
Kazanorgsintez PE80B-275 Medium Density Polyethylene Composite Production Method: Copolymerization of ethylene at low pressure using advanced technology and in presence of complex catalysts on carrier material that allows production of polyethylene with enhanc.. |
|||
Density | 0.945 - 0.953 g/cc @Temperature 20.0 °C |
0.0341 - 0.0344 lb/in³ @Temperature 68.0 °F |
|
Kazanorgsintez PE80B-275 Medium Density Polyethylene Composite Production Method: Copolymerization of ethylene at low pressure using advanced technology and in presence of complex catalysts on carrier material that allows production of polyethylene with enhanc.. |
|||
Density | 0.943 - 0.951 g/cc @Temperature 23.0 °C |
0.0341 - 0.0344 lb/in³ @Temperature 73.4 °F |
|
Kazanorgsintez PE80B-286 Medium Density Polyethylene Composite Production Method: Copolymerization of ethylene at low pressure using advanced technology and in presence of complex catalysts on carrier material that allows production of polyethylene with enhanc.. |
|||
Density | 0.945 - 0.953 g/cc @Temperature 20.0 °C |
0.0341 - 0.0344 lb/in³ @Temperature 68.0 °F |
|
Kazanorgsintez PE80B-286 Medium Density Polyethylene Composite Production Method: Copolymerization of ethylene at low pressure using advanced technology and in presence of complex catalysts on carrier material that allows production of polyethylene with enhanc.. |