Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.05 g/cc @Temperature 60.0 °C |
0.0379 lb/in³ @Temperature 140 °F |
|
BASF Pluracol® 922 Rigid Polyol Description: Pluracol® 922 polyol is an aromatic initiator-based polyol for rigid foams developed for use in spray formulations, or in polyol blends that can utilize its inherent fast reactivity. P.. |
|||
Density | 1.05 g/cc @Temperature 25.0 °C |
0.0379 lb/in³ @Temperature 77.0 °F |
|
BASF Pluracol® GP 430R Specialty Polyol Description: Pluracol® GP polyols are a series of four trifunctional polyols formed by adding propylene oxide to a glycerine nucleus. All Pluracol GP polyols are used in the preparation of polyure.. |
|||
Density | 1.05 g/cc @Temperature 25.0 °C |
0.0379 lb/in³ @Temperature 77.0 °F |
|
BASF Pluracol® 5250 Graft Slabstock Foam Polyol Description: Pluracol® 5250 polyol is a graft polyether triol containing copolymerized styrene and acrylonitrile. This secondary hydroxyl-terminated polyol contains approximately 50% solids. It is .. |
|||
Density | 1.05 g/cc @Temperature 60.0 °C |
0.0379 lb/in³ @Temperature 140 °F |
|
BASF Pluracol® SG-360 Rigid Polyol Description: Pluracol® SG-360 polyol is a clear, light colored, low viscosity, sucrose/glycerine polyol. Pluracol SG-360 contains no nitrogen. The medium functionality polyol, when combined with su.. |