Physical Properties Metric English Comments
Density 1.09 - 1.13 g/cc

@Temperature 20.0 °C
0.0394 - 0.0408 lb/in³

@Temperature 68.0 °F
A Grade, 1st Quality
Kazanorgsintez Purified Polyglycol
Production Method: A Grade - Glycol solution in water with mass fraction greater than 75% B Grade - Glycol solution in water with mass fraction greater than 45% Application: A Grade - Intended for ..