Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.216 g/cc @Temperature 100 °C |
0.04393 lb/in³ @Temperature 212 °F |
Concentration 0.28 kg FeCl3/kg |
Solvay Chemicals Ferric chloride Ferric chloride is a red brown aqueous solution, with a slight odor.EINECS: 231-729-4/CAS: 7705-08-0/UN: 2582Information provided by Solvay |