Polymer Property : Density = 0.04776 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 1.322 g/cc

@Temperature 0.000 °C
0.04776 lb/in³

@Temperature 32.0 °F
Concentration 0.32 kg FeCl3/kg
Solvay Chemicals Ferric chloride
Ferric chloride is a red brown aqueous solution, with a slight odor.EINECS: 231-729-4/CAS: 7705-08-0/UN: 2582Information provided by Solvay