Polymer Property : Density = 0.650 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 0.650 g/cc

@Temperature 22.0 °C
0.0235 lb/in³

@Temperature 71.6 °F
Cure Cycle: 5 days at 22°C; ASTM D792
Hexcel® Redux® 830 Two-Part Epoxy Syntactic Paste Adhesive
Redux® 830 is a low density, self-extinguishing, syntactic, room temperature curing, two-part, epoxy paste adhesive. Redux® 830 is supplied as a 1.5 working kit.Features: Low density; Self-extingu..
Density 0.650 g/cc

@Temperature 316 °C
0.0235 lb/in³

@Temperature 600 °F
Duratherm 630 Paraffinic Heat Transfer Fluid
Duratherm 630 - rated to 630°F it has the highest rated bulk temperature of petroleum based thermal fluids. Duratherm 630 is engineered for applications requiring high temperature stability (630°F..