Physical Properties Metric English Comments
Density 0.720 g/cc

@Temperature 25.0 °C
0.0260 lb/in³

@Temperature 77.0 °F
Part A, Uncured; ASTM D1875-69
Hexcel® Redux® 830 Two-Part Epoxy Syntactic Paste Adhesive
Redux® 830 is a low density, self-extinguishing, syntactic, room temperature curing, two-part, epoxy paste adhesive. Redux® 830 is supplied as a 1.5 working kit.Features: Low density; Self-extingu..