Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.8084 g/cc @Pressure 0.6201 MPa, Temperature 110 °C |
0.02921 lb/in³ @Pressure 89.94 psi, Temperature 230 °F |
|
Solvay Chemicals Allyl chloride 3-chloropropene Allyl chloride is mainly used in the manufacture of epichlorohydrin. It is also used in the production of allylic ethers, esters, silanes and quaternary ammonium derivatives.EINECS Number: 203-457-6.. |
|||
Density | 0.8084 g/cc @Pressure 0.6201 MPa, Temperature 110 °C |
0.02921 lb/in³ @Pressure 89.94 psi, Temperature 230 °F |
|
Solvay Chemicals Allyl chloride High purity – Non stabilized 3-chloropropene Allyl chloride is mainly used in the manufacture of epichlorohydrin. It is also used in the production of allylic ethers, esters, silanes and quaternary ammonium derivatives.EINECS Number: 203-457-6.. |
|||
Density | 0.8084 g/cc @Pressure 0.6201 MPa, Temperature 110 °C |
0.02921 lb/in³ @Pressure 89.94 psi, Temperature 230 °F |
|
Solvay Chemicals Allyl chloride High purity 3-chloropropene Allyl chloride is mainly used in the manufacture of epichlorohydrin. It is also used in the production of allylic ethers, esters, silanes and quaternary ammonium derivatives.EINECS Number: 203-457-6.. |