Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.827 g/cc @Temperature 15.6 °C |
0.0299 lb/in³ @Temperature 60.0 °F |
|
Paratherm Corporation Paratherm™ CR Heat Transfer Fluid Paratherm CR® heat transfer fluid is a blend of synthetic components formulated to provide superior cooling performance in closed-loop heat-transfer systems operating down to -88°C (-127°F) yet i.. |
|||
Density | 0.827 g/cc @Temperature -73.3 °C |
0.0299 lb/in³ @Temperature -100 °F |
|
Paratherm Corporation Paratherm™ LR Heat Transfer Fluid Paratherm LR™ heat transfer fluid is an aliphatic-hydrocarbon based heat transfer fluid designed for use in closed-loop, liquid phase heating and cooling systems up to 450°F in electric and steam .. |