Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.9709 g/cc @Pressure 0.0124 MPa, Temperature -5.00 °C |
0.03508 lb/in³ @Pressure 1.80 psi, Temperature 23.0 °F |
|
Solvay Chemicals Allyl chloride 3-chloropropene Allyl chloride is mainly used in the manufacture of epichlorohydrin. It is also used in the production of allylic ethers, esters, silanes and quaternary ammonium derivatives.EINECS Number: 203-457-6.. |
|||
Density | 0.9709 g/cc @Pressure 0.0124 MPa, Temperature -5.00 °C |
0.03508 lb/in³ @Pressure 1.80 psi, Temperature 23.0 °F |
|
Solvay Chemicals Allyl chloride High purity – Non stabilized 3-chloropropene Allyl chloride is mainly used in the manufacture of epichlorohydrin. It is also used in the production of allylic ethers, esters, silanes and quaternary ammonium derivatives.EINECS Number: 203-457-6.. |
|||
Density | 0.9709 g/cc @Pressure 0.0124 MPa, Temperature -5.00 °C |
0.03508 lb/in³ @Pressure 1.80 psi, Temperature 23.0 °F |
|
Solvay Chemicals Allyl chloride High purity 3-chloropropene Allyl chloride is mainly used in the manufacture of epichlorohydrin. It is also used in the production of allylic ethers, esters, silanes and quaternary ammonium derivatives.EINECS Number: 203-457-6.. |