Polymer Property : Density = 1.015 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 1.015 - 1.018 g/cc

@Temperature 20.0 °C
0.03667 - 0.03678 lb/in³

@Temperature 68.0 °F
Highest Class, First Class
Kazanorgsintez Monoethanolamine
Production Method: Interaction of ammonia or its water solution with ethylene oxide. Application: Used in the gas and petroleum industry for absorption of acid gases and sulfur-containing organic co..
Density 1.015 - 1.025 g/cc

@Temperature 20.0 °C
0.03667 - 0.03703 lb/in³

@Temperature 68.0 °F
Second Class
Kazanorgsintez Monoethanolamine
Production Method: Interaction of ammonia or its water solution with ethylene oxide. Application: Used in the gas and petroleum industry for absorption of acid gases and sulfur-containing organic co..
Density 1.015 - 1.05 g/cc

@Temperature 20.0 °C
0.03667 - 0.0379 lb/in³

@Temperature 68.0 °F
Third Class
Kazanorgsintez Monoethanolamine
Production Method: Interaction of ammonia or its water solution with ethylene oxide. Application: Used in the gas and petroleum industry for absorption of acid gases and sulfur-containing organic co..