Density 1.067 g/cc

@Temperature 110 °C
0.03855 lb/in³

@Temperature 230 °F
Solvay Chemicals Epichlorohydrin
Epichlorohydrin is a chemical intermediate, mainly dedicated to the manufacturing of epoxy resins used in Paints & coatings, Composites, Adhesives and Electronics. It is also used in non-epoxy appli..
Density 1.067 g/cc

@Temperature 25.0 °C
0.03855 lb/in³

@Temperature 77.0 °F
BASF Pluracol® 1168 Rigid Polyol
Description: Pluracol® 1168 Polyol is a general purpose aromatic initiator-based polyol for rigid foams for use in a variety of applications. It is attractively priced for consideration for foaming..