Polymer Property : Density = 1.075 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 1.075 g/cc

@Temperature 25.0 °C
0.03884 lb/in³

@Temperature 77.0 °F
BASF Pluracol® 1578 Rigid Polyol
Description: Pluracol® 1578 polyol is a general purpose aromatic initiator-based polyol for rigid foams for use in a variety of applications. It is attractively priced for consideration for foaming..