Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity Measure | 440 cSt @Temperature 37.8 °C |
440 cSt @Temperature 100 °F |
|
Dow VORANOL™ 4703 Polyether Polyol VORANOL™ 4703 polyether polyol is a nominal 5000 molecular weight, high reactivity capped triol. It has a high primary hydroxyl content making it suitable for use in making all types of high resil.. |