Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity Measure | 470 - 515 cSt @Temperature 25.0 °C |
470 - 515 cSt @Temperature 77.0 °F |
ASTM D445-94 |
Dow VORANOL™ CP 3131 Polyol VORANOL™ CP 3131 polyol is a low to medium reactivity polyether triol, especially designed for the production of hot molded polyurethane flexible foams.Information provided by Dow |