Physical Properties Metric English Comments
Vapor Pressure 0.0000867 bar

@Temperature 150 °C
0.0650 torr

@Temperature 302 °F
ChevronTexaco 22 Heat Transfer Oil
FeaturesChevron Heat Transfer Oils are mineral-type transfer oils for use in secondary or indirect heating systems. They are formulated with ISOSYN® base stocks. Chevron Heat Transfer Oils are nont..