Polymer Property : Vapor Pressure = 0.000900 bar Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Vapor Pressure 0.000900 bar

@Temperature 0.000 °C
0.675 torr

@Temperature 32.0 °F
BASF Glacial Acrylic Acid
Formula: C3H4O2CAS: 79-10-7Description: Acrylic acid glacial is a colorless liquid having a sharp, acrid odor. It is completely soluble in water. Acrylic acid is a monomer used in industrial synthes..