Polymer Property : Vapor Pressure = 0.108 bar Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Vapor Pressure 0.108 bar

@Temperature 135 °C
81.0 torr

@Temperature 275 °F
Paratherm Corporation Paratherm™ LR Heat Transfer Fluid
Paratherm LR™ heat transfer fluid is an aliphatic-hydrocarbon based heat transfer fluid designed for use in closed-loop, liquid phase heating and cooling systems up to 450°F in electric and steam ..