Physical Properties | Metric | English | Comments |
---|---|---|---|
Vapor Pressure | 0.130 bar @Temperature 10.0 °C |
97.5 torr @Temperature 50.0 °F |
|
Solvay Chemicals A20 Chloroform Chloroform is a non-flammable product.EINECS Number: 200-663-8/CAS Number: 67-66-3/UN number: 1888Information provided by Solvay |
|||
Vapor Pressure | 0.130 bar @Temperature 10.0 °C |
97.5 torr @Temperature 50.0 °F |
|
Solvay Chemicals E9000 Chloroform Chloroform is a non-flammable product.EINECS Number: 200-663-8/CAS Number: 67-66-3/UN number: 1888Information provided by Solvay |
|||
Vapor Pressure | 0.130 bar @Temperature 60.0 °C |
97.5 torr @Temperature 140 °F |
Concentration 0.20 kg HCl/kg |
Solvay Chemicals Hydrochloric Acid 31% - Technical Grade (11 wt% - 20 wt% Concentration) Hydrochloric acid, also known as muriatic acid, is a colorless to yellow liquid, with a pungent odor. Hydrochloric acid is a strong acid used as chemical reagent, pH-regulating, ion exchanger regene.. |