Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Vapor Pressure 0.000669 bar

@Temperature 204 °C
0.502 torr

@Temperature 400 °F
Paratherm Corporation Paratherm™ HE Heat Transfer Fluid
Paratherm HE® is a high flash and fire point heat transfer fluid. Engineered for higher thermal and oxidative stability, it is efficient and cost effective. Its greater purity allows it to strong..