Polymer Property : Vapor Pressure = 0.959 bar Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Vapor Pressure 0.959 bar

@Temperature 177 °C
719 torr

@Temperature 350 °F
Paratherm Corporation Paratherm™ CR Heat Transfer Fluid
Paratherm CR® heat transfer fluid is a blend of synthetic components formulated to provide superior cooling performance in closed-loop heat-transfer systems operating down to -88°C (-127°F) yet i..