Vapor Pressure 0.0213 bar

@Temperature 300 °C
16.0 torr

@Temperature 572 °F
ChevronTexaco 46 Heat Transfer Oil
FeaturesChevron Heat Transfer Oils are mineral-type transfer oils for use in secondary or indirect heating systems. They are formulated with ISOSYN® base stocks. Chevron Heat Transfer Oils are nont..
Vapor Pressure 0.0213 bar

@Temperature 300 °C
16.0 torr

@Temperature 572 °F
ChevronTexaco Texatherm®
Texaco Texatherm and Texatherm 22 deliver value through:Excellent thermal efficiency and stability — Long oil life is assured by outstanding thermal and oxidation stability which prevents sludging ..
Vapor Pressure 0.0213 bar

@Temperature 135 °C
16.0 torr

@Temperature 275 °F
AboCure
Abatron AboCast/AboCure 8109-7
Processing: 100/80 pbw; Potlife: 6-7 days/20°C (68°F), 12-24 h/40°C (105°F), 0.75-7 h /60°C (140°F); mix at 50-80°C (120-175°F); cures in: 1 h/100°C (212°F) + 4 h/150°C (300°F) postcure...