Physical Properties Metric English Comments
Vapor Pressure 2.67e-7 bar

@Temperature 100 °C
0.000200 torr

@Temperature 212 °F
ChevronTexaco 46 Heat Transfer Oil
FeaturesChevron Heat Transfer Oils are mineral-type transfer oils for use in secondary or indirect heating systems. They are formulated with ISOSYN® base stocks. Chevron Heat Transfer Oils are nont..
Vapor Pressure 2.67e-7 bar

@Temperature 100 °C
0.000200 torr

@Temperature 212 °F
ChevronTexaco Texatherm®
Texaco Texatherm and Texatherm 22 deliver value through:Excellent thermal efficiency and stability — Long oil life is assured by outstanding thermal and oxidation stability which prevents sludging ..
Vapor Pressure 2.67e-7 bar

@Temperature 100 °C
0.000200 torr

@Temperature 212 °F
Knudsen
Solvay Specialty Polymers FOMBLIN® Y H-VAC 18/8 PFPE Pump Oil
FOMBLIN Y fluids are a mixture of fluorinated polymers obtained by a photochemical process that begins with hexafluoropropylene. Since the FOMBLIN chemical chain contains only carbon, fluorine, and..