Physical Properties Metric English Comments
Vapor Pressure 0.285 bar

@Temperature 80.0 °C
214 torr

@Temperature 176 °F
898 g/m<sup>3</sup> concentration of saturated vapor
Solvay Chemicals Epichlorohydrin
Epichlorohydrin is a chemical intermediate, mainly dedicated to the manufacturing of epoxy resins used in Paints & coatings, Composites, Adhesives and Electronics. It is also used in non-epoxy appli..