Physical Properties Metric English Comments
Vapor Pressure 0.06964 bar

@Temperature 316 °C
52.23 torr

@Temperature 600 °F
Duratherm S Silicone Heat Transfer Fluid
Duratherm S - a silicone based heat transfer fluid that is ideally suited for high oxidation or completely exposed systems up to 650°F. Duratherm S is virtually impervious to oxidation and offers s..