Polymer Property : Vapor Pressure = 6.00e-12 torr Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Vapor Pressure 8.00e-15 bar

@Temperature 20.0 °C
6.00e-12 torr

@Temperature 68.0 °F
Knudsen
Solvay Specialty Polymers FOMBLIN® Y H-VAC 40/11 PFPE Pump Oil
FOMBLIN Y fluids are a mixture of fluorinated polymers obtained by a photochemical process that begins with hexafluoropropylene. Since the FOMBLIN chemical chain contains only carbon, fluorine, and..