Physical Properties | Metric | English | Comments |
---|---|---|---|
Solubility | 95 ppm | 95 ppm | |
3M Novec™ 7100DL Engineered Fluid A higher purity version of 3M™ Novec™ 7100, 3M™ Novec™ 7100DL is tightly-controlled for ions, metals and non-volatile residue. It is used in precision cleaning and deposition applications when h.. |