Polymer Property : Linear Mold Shrinkage, Flow = 0.0024 cm/cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Flow 0.0021 - 0.0024 cm/cm

@Time 86400 sec
0.0021 - 0.0024 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP LUBRICOMP EFL36 PEI
LNP LUBRICOMP* EFL36 is a compound based on Polyetherimide resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Internally Lubricated.
Linear Mold Shrinkage, Flow 0.0021 - 0.0024 cm/cm

@Time 86400 sec
0.0021 - 0.0024 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP LUBRICOMP EFL36 PEI (Asia Pacific)
LNP LUBRICOMP* EFL36 is a compound based on Polyetherimide resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated.
Linear Mold Shrinkage, Flow 0.0021 - 0.0024 cm/cm

@Time 86400 sec
0.0021 - 0.0024 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP LUBRICOMP EFL36 PEI (Europe-Africa-Middle East)
LNP LUBRICOMP* EFL36 is a compound based on Polyetherimide resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated.
Linear Mold Shrinkage, Flow 0.0021 - 0.0024 cm/cm

@Time 86400 sec
0.0021 - 0.0024 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP LUBRICOMP EFL36XXC PEI
LNP* Lubricomp* EFL36XXC is a compound based on Polyetherimide containing 30% Glass Fiber, 155 PTFE. Characteristics of this grade are: Internally Lubricated.