Polymer Property : Linear Mold Shrinkage, Flow = 0.0053 cm/cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Flow 0.0053 cm/cm

@Time 86400 sec
0.0053 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP LUBRICOMP RFL36L PA 66
LNP* LUBRICOMP* RFL36L is a compound based on Nylon 66 resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Wear Resistant, Low Extractible.
Linear Mold Shrinkage, Flow 0.0053 cm/cm

@Time 86400 sec
0.0053 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP LUBRICOMP RFL36L PA 66 (Asia Pacific)
LNP* Lubricomp* RFL36L is a compound based on Nylon 66 resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated, Low Extractible.
Linear Mold Shrinkage, Flow 0.0053 cm/cm

@Time 86400 sec
0.0053 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP Lubriloy D20001 PC
LNP LUBRILOY* D20001 is a compound based on Polycarbonate resin containing Flame Retardant, Proprietary Lubricant. Added features of this material include: Flame Retardant.This data was supplied by..
Linear Mold Shrinkage, Flow 0.0053 cm/cm

@Time 86400 sec
0.0053 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP LUBRILOY D20001 PC (Asia Pacific)
LNP LUBRILOY* D20001 is a compound based on Polycarbonate resin containing Flame Retardant, Proprietary Lubricant. Added features of this material include: Flame Retardant.