Linear Mold Shrinkage, Flow 0.0059 cm/cm

@Time 86400 sec
0.0059 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP LUBRICOMP DL004 PC
LNP* Lubricomp* DL004 is a compound based on Polycarbonate resin containing 20% PTFE. Added features of this material include: Internally Lubricated.
Linear Mold Shrinkage, Flow 0.0059 cm/cm

@Time 86400 sec
0.0059 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP LUBRICOMP DL004 PC (Asia Pacific)
LNP* Lubricomp* DL004 is a compound based on Polycarbonate resin containing PTFE. Added features of this material include: Internally Lubricated.
Linear Mold Shrinkage, Flow 0.0059 cm/cm

@Time 86400 sec
0.0059 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP THERMOCOMP DB0049F PC
LNP* THERMOCOMP* DB0049F is a compound based on Polycarbonate resin containing 20% Glass Bead. Added features of this material include: Flame Retardant, Superior Molding.
Linear Mold Shrinkage, Flow 0.0059 cm/cm

@Time 86400 sec
0.0059 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP THERMOCOMP DB0049F PC (Asia Pacific)
LNP* Thermocomp* DB0049F is a compound based on Polycarbonate resin containing Glass Bead, Flame Retardant. Added features of this material include: Flame Retardant, Superior Molding.
Linear Mold Shrinkage, Flow 0.0059 cm/cm

@Time 86400 sec
0.0059 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP LUBRICOMP DL004XXC PC
LNP* LUBRICOMP* DL004XXC is a compound based on Polycarbonate containing 20% PTFE. Characteristics of this grade are: Interrnally Lubricated.