Linear Mold Shrinkage, Flow 0.0065 cm/cm

@Time 86400 sec
0.0065 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP COLORCOMP D1000P PC
LNP* COLORCOMP* D1000P is an unfilled Polycarbonate. Added feature of this grade is: Exceptional Processing.
Linear Mold Shrinkage, Flow 0.0065 cm/cm

@Time 86400 sec
0.0065 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP COLORCOMP D1000P PC (Asia Pacific)
LNP* Colorcomp* D1000P is a compound based on Polycarbonate resin containing Unfilled Custom Color. Added features of this material include: Exceptional Processing.
Linear Mold Shrinkage, Flow 0.0065 cm/cm

@Time 86400 sec
0.0065 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP THERMOCOMP MF006S PP
LNP* THERMOCOMP* MF006S is a compound based on Polypropylene resin containing 30% Glass Fiber. Added features of this material include: Heat Stabilized.
Linear Mold Shrinkage, Flow 0.0065 cm/cm

@Time 86400 sec
0.0065 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP Thermocomp 2C004
LNP THERMOCOMP* 2C004 is a compound based on Ethylene Tetrafluoroethylene Copolymer resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was sup..
Linear Mold Shrinkage, Flow 0.0065 cm/cm

@Time 86400 sec
0.0065 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP THERMOCOMP 2C004 ETFE
LNP* THERMOCOMP* 2C004 is a compound based on ETFE resin containing 20% Carbon Fiber. Added features of this material include: Electrically Conductive.
Linear Mold Shrinkage, Flow 0.0065 cm/cm

@Time 86400 sec
0.0065 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP Thermocomp MF006S PP (Asia Pacific)
LNP* Thermocomp* MF006S is a compound based on Polypropylene resin containing Glass Fiber. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for the Asia P..
Linear Mold Shrinkage, Flow 0.0065 cm/cm

@Time 86400 sec
0.0065 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP THERMOCOMP MF006SU PP
LNP* THERMOCOMP* MF006SU is a compound based on Polypropylene containing 30% lass Fiber. Characteristics of this grade are: Heat Stabilized, Chemically Coupled, UV Stabilized.