Physical Properties Metric English Comments
Linear Mold Shrinkage, Flow 0.0108 cm/cm

@Time 86400 sec
0.0108 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP LUBRICOMP KFL32R Acetal Copolymer
LNP LUBRICOMP* KFL32R is a compound based on Acetal Copolymer resin containing 10% Glass Fiber, 15% PTFE. Added feature of this material is: Easy Release, Wear Resistant.
Linear Mold Shrinkage, Flow 0.0108 cm/cm

@Time 86400 sec
0.0108 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP THERMOCOMP PH0320A PA 6 (Asia Pacific)
LNP THERMOCOMP* PH0320A is a compound based on Nylon 6 resin. Added features of this material include: High Specific Gravity.
Linear Mold Shrinkage, Flow 0.0108 cm/cm

@Time 86400 sec
0.0108 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP THERMOCOMP PH0320A PA 6
LNP THERMOCOMP* PH0320A is a compound based on Nylon 6 resin. Added features of this material include: High Specific Gravity.