Polymer Property : Linear Mold Shrinkage, Flow = 0.016 in/in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Flow 0.016 cm/cm

@Time 86400 sec
0.016 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP LUBRICOMP YL003C Polyester Elastomer
LUBRICOMP* YL003C is a compound based on Polyester Elastomer resin containing 15% PTFE. Added features of this grade include: Clean Compound System, Wear Resistant.
Linear Mold Shrinkage, Flow 0.016 cm/cm

@Time 86400 sec
0.016 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP LUBRICOMP YL003C Polyester Elastomer (Asia Pacific)
LUBRICOMP* YL-4030 CCS is a PTFE Lubricated Compound based on Polyester Elastomer resin which has low ionic and low outgassing performance for the Semicon and Internal Hard Disk Drive applications.
Linear Mold Shrinkage, Flow 0.016 - 0.018 cm/cm

@Time 86400 sec
0.016 - 0.018 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP LUBRILOY U2000A PPA
LNP* LUBRILOY* U2000A is a compound based on Polyphthalamide resin containing Proprietary Lubricant. Added feature of this material is: Wear Resistant.
Linear Mold Shrinkage, Flow 0.016 - 0.018 cm/cm

@Time 86400 sec
0.016 - 0.018 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP LUBRILOY U2000A PPA (Asia Pacific)
LNP* Lubriloy* U2000A is a compound based on Polyphthalamide resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated.
Linear Mold Shrinkage, Flow 0.016 - 0.018 cm/cm

@Time 86400 sec
0.016 - 0.018 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP STAT-KON MD000IS PP
LNP STAT-KON* MD000IS is a compound based on Polypropylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact.
Linear Mold Shrinkage, Flow 0.016 - 0.018 cm/cm

@Time 86400 sec
0.016 - 0.018 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP STAT-KON MD000IS PP
LNP STAT-KON* MD000IS is a compound based on Polypropylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact.
Linear Mold Shrinkage, Flow 0.016 - 0.018 cm/cm

@Time 86400 sec
0.016 - 0.018 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP STAT-KON MD000ISC PP (Asia Pacific)
LNP STAT-KON* MD000ISC is a compound based on Polypropylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive.
Linear Mold Shrinkage, Flow 0.016 - 0.018 cm/cm

@Time 86400 sec
0.016 - 0.018 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP STAT-KON MD000ISC PP (Asia Pacific)
LNP STAT-KON* MD000ISC is a compound based on Polypropylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive.
Linear Mold Shrinkage, Flow 0.016 - 0.018 cm/cm

@Time 86400 sec
0.016 - 0.018 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP THERMOCOMP KF002L Acetal Homopoly
LNP* THERMOCOMP* KF002L is a compound based on Acetal Homopolymer resin containing 10% Glass Fiber. Added features of this material include: Low Extractible.
Linear Mold Shrinkage, Flow 0.016 - 0.018 cm/cm

@Time 86400 sec
0.016 - 0.018 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP THERMOCOMP KF002L Acetal Homopoly (Asia Pacific)
LNP* Thermocomp* KF002L is a compound based on Acetal Homopolymer resin containing Glass Fiber. Added features of this material include: Low Extractible.
Linear Mold Shrinkage, Flow 0.016 cm/cm

@Time 86400 sec
0.016 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP THERMOCOMP MH0500C PP (Asia Pacific)
LNP* Thermocomp* MH0500C is a compound based on Polypropylene resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity.
Linear Mold Shrinkage, Flow 0.016 cm/cm

@Time 86400 sec
0.016 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP THERMOCOMP MH0500C PP
LNP* THERMOCOMP* MH0500C is a compound based on Polypropylene resin. Added feature of this material is: High Specific Gravity.
Linear Mold Shrinkage, Flow 0.016 - 0.018 cm/cm

@Time 86400 sec
0.016 - 0.018 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP STAT-KON MD000ISC PP
LNP STAT-KON* MD000ISC is a compound based on Polypropylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact.
Linear Mold Shrinkage, Flow 0.016 - 0.018 cm/cm

@Time 86400 sec
0.016 - 0.018 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP STAT-KON MD000ISC PP
LNP STAT-KON* MD000ISC is a compound based on Polypropylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact.
Linear Mold Shrinkage, Flow 0.016 - 0.018 cm/cm

@Time 86400 sec
0.016 - 0.018 in/in

@Time 24.0 hour
ASTM D 955
SABIC Innovative Plastics LNP Stat-kon MD000IU PP
LNP* Stat-kon* MD000IU is a compound based on Polypropylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact, UV Stabilized.This data wa..
Linear Mold Shrinkage, Flow 0.016 - 0.018 cm/cm

@Time 86400 sec
0.016 - 0.018 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP Stat-kon MD000IU PP
LNP* Stat-kon* MD000IU is a compound based on Polypropylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact, UV Stabilized.This data wa..
Linear Mold Shrinkage, Flow 0.016 - 0.018 cm/cm

@Time 86400 sec
0.016 - 0.018 in/in

@Time 24.0 hour
ASTM D 955
SABIC Innovative Plastics LNP Stat-kon MD000IU PP (Asia Pacific)
LNP* Stat-kon* MD000IU is a compound based on Polypropylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact, UV Stabilized.This data wa..
Linear Mold Shrinkage, Flow 0.016 - 0.018 cm/cm

@Time 86400 sec
0.016 - 0.018 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP Stat-kon MD000IU PP (Asia Pacific)
LNP* Stat-kon* MD000IU is a compound based on Polypropylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact, UV Stabilized.This data wa..