Polymer Property : Linear Mold Shrinkage, Flow = 0.020 cm/cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Flow 0.018 - 0.020 cm/cm

@Time 86400 sec
0.018 - 0.020 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP THERMOCOMP RB008 PA 66 (Asia Pacific)
LNP THERMOCOMP* RB008 is a compound based on Nylon 66 resin containing Glass Bead.
Linear Mold Shrinkage, Flow 0.018 - 0.020 cm/cm

@Time 86400 sec
0.018 - 0.020 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP THERMOCOMP RB008 PA 66 (Asia Pacific)
LNP THERMOCOMP* RB008 is a compound based on Nylon 66 resin containing Glass Bead.
Linear Mold Shrinkage, Flow 0.018 - 0.020 cm/cm

@Time 86400 sec
0.018 - 0.020 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP THERMOCOMP RB008 PA 66
LNP THERMOCOMP* RB008 is a compound based on Nylon 66 resin containing 40% Glass Bead.
Linear Mold Shrinkage, Flow 0.018 - 0.020 cm/cm

@Time 86400 sec
0.018 - 0.020 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP THERMOCOMP RB008 PA 66
LNP THERMOCOMP* RB008 is a compound based on Nylon 66 resin containing 40% Glass Bead.