Critical Temperature 101.1 °C
214.0 °F
Solvay Specialty Polymers Meforex® 134a Ozone-Friendly CFC Replacement
Formula: CH2FCF3; Name: 1,1,1,2 Tetrafluoroethane. Replaces CFC 12, R 500. Domestic refrigeration, commercial and automotive air-conditioning, polystyrene and polyurethanes foams, and pharmaceutic..