Polymer Property : Critical Temperature = 29.7 °C Product List

Chemical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Chemical Properties Metric English Comments
Critical Temperature 29.7 °C
85.5 °F
Shandong Dongyue Shenzhou New Material Co Vinylidene Fluoride (VDF)
Conformable with: Q/DYS 007-2007VDF is a kind of colorless gas under normal temperature and pressure, nontoxic, flammable, with little ether odor. It has the common gender of alkene, and can be pol..