Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Critical Temperature = 559 °F Product List

Chemical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Chemical Properties Metric English Comments
Critical Temperature 293 °C
559 °F
Estimated
3M Fluorinert™ FC-43 Electronic Liquid
3M™ Fluorinert™ Liquid FC-43 is a non-conductive, thermally and chemically stable liquid ideal for many single phase heat transfer fluid applications, especially in the electronics and semiconduct..