Chemical Properties | Metric | English | Comments |
---|---|---|---|
Critical Temperature | 743 °C | 1370 °F | Ar3 |
Latrobe LSSâ„¢ 4140 Alloy Steel (AISI 4140) TLS 4140 and 4142HT are versatile, alloy steels which are used in variety of tooling and other industrial applications. TLS 4140 is the classic AISI 4140 alloy steel which is sold in the annealed co.. |
|||
Critical Temperature | 743 °C | 1370 °F | Ar3 |
Latrobe LSSâ„¢ 4142 Alloy Steel (AISI 4142) TLS 4140 and 4142HT are versatile, alloy steels which are used in variety of tooling and other industrial applications. TLS 4140 is the classic AISI 4140 alloy steel which is sold in the annealed co.. |
|||
Critical Temperature | 743 °C | 1370 °F | Ar3 |
Latrobe LSSâ„¢ D3 Tool Steel (ASTM D3) TLS D3 tool steel is a high-carbon, high-chromium, oil-hardening tool steel that is characterized by a relatively high attainable hardness and numerous, large, chromium-rich alloy carbides in the mi.. |
|||
Critical Temperature | 743 °C | 1370 °F | |
Crucible Steel KETOS® Tool Steel, AISI O1 Ketos is an oil-hardening tool steel which may be hardened from fairly low temperatures with little size change. This grade combines deep-hardening qualities with a fine-grained structure, affording.. |