Chemical Properties | Metric | English | Comments |
---|---|---|---|
Critical Temperature | 780 °C | 1440 °F | Ac2 |
QuesTek® Innovations Ferrium® S53® Corrosion Resistant High Strength Steel for Aerospace Structural Applications Description: Ferrium® S53® is a corrosion resistant ultra high-strength steel for structural aerospace applications. Ferrium® S53® was designed to provide mechanical properties equal to, or bett.. |
|||
Critical Temperature | 780 °C | 1440 °F | Ar1 |
Latrobe Tatmo-VN™ ASTM M7 High Speed Steel TATMO-VN is an M7 type high speed steel modified by alloy balancing and a nitrogen addition to develop superior hardness response in heat treatment. It is an excellent grade for
many cutting tool ap.. |