Critical Temperature 818.3 °C
1505 °F
Crucible Steel HALCOMB® 218 Tool Steel, AISI H11
Halcomb 218 is a general purpose hot work tool steel, combining good toughness with moderate high-temperature strength and heat check resistance. Because of its high toughness, it is particularly su..