Chemical Properties | Metric | English | Comments |
---|---|---|---|
Critical Temperature | 830 °C | 1530 °F | Ac1 |
Latrobe HS-29XLâ„¢ ASTM M2-HC High Speed Steel HS-29XL (M2-HC) is the M2 composition with the carbon content increased and with the addition of alloy sulfides. The higher carbon content provides higher hardness and
superior red hardness compared.. |
|||
Critical Temperature | 830 °C | 1530 °F | Ac1 |
Latrobe LSSâ„¢ H10 Hot Work Tool Steel (ASTM H10) TLS H10 hot work tool steel is a chromium-molybdenum hot work steel that exhibits excellent resistance to softening at elevated temperature. This grade is very resistant to thermal fatigue cracking .. |
|||
Critical Temperature | 830 °C | 1530 °F | Ac1 |
Latrobe LSSâ„¢ H10A Modified TLS H10 Mod. hot work tool steel is a chromium-molybdenum H10-type hot work steel which contains cobalt for increased strength and resistance to softening at elevated temperature. This grade is also.. |
|||
Critical Temperature | 830 °C | 1530 °F | Ac1 |
Latrobe LSSâ„¢ H11 Hot Work Tool Steel (ASTM H11) TLS H11 hot work tool steel is a 5% chromium hot work steel that is characterized by excellent impact toughness. It contains less vanadium than the widely-used H13 hot work tool steel. This provides.. |
|||
Critical Temperature | 830 °C | 1530 °F | Ac1 |
Latrobe TNWâ„¢ ASTM M10 High Speed Steel TNW is an M10 type high speed steel with a composition that combines the high toughness of a high-molybdenum steel and the excellent wear resistance provided by the 2%
vanadium content. TNW is popul.. |