Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Critical Temperature = 866 °C Product List

Chemical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Chemical Properties Metric English Comments
Critical Temperature 866 °C
1590 °F
Ac1
Latrobe DuraTechâ„¢ NINE Powder Metal Tool Steel
DuraTech NINE is an air-hardening, powder metal tool steel that provides very high wear resistance in combination with high impact toughness. A large volume of hard vanadium carbides provides the hi..