Chemical Properties | Metric | English | Comments |
---|---|---|---|
Ionic Impurities - Na (Sodium) | 17 ppm | 17 ppm | |
Epoxy Technology EPO-TEK® 354 High Temperature Epoxy Product Description: EPO-TEK® 354 is a two component, high Tg epoxy designed for semiconductor packaging in medical, fiber optic and optoelectronic assemblies. It is an electrically and thermally i.. |
|||
Ionic Impurities - Na (Sodium) | 17 ppm | 17 ppm | |
Epoxy Technology EPO-TEK® E3035 Electrically Conductive Adhesive Product Description: EPO-TEK® E3035 is a single component, silver-filled epoxy for hybrid die and component attach.Advantages & Application Notes: Performs exceptionally well as a die attach for sm.. |