Polymer Property : Ionic Impurities - Na (Sodium) = 22 ppm Product List

Chemical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Chemical Properties Metric English Comments
Ionic Impurities - Na (Sodium) 22 ppm
22 ppm
Epoxy Technology EPO-TEK® E3037 Epoxy
Material Description: A single component, electrically conductive, thixotropic silver-filled epoxy for die-attach and SMD-attach inside hybrid microelectronics.Information Provided by Epoxy Technolo..