Chemical Properties | Metric | English | Comments |
---|---|---|---|
Ionic Impurities - Na (Sodium) | 52 ppm | 52 ppm | |
Epoxy Technology EPO-TEK® 353ND Black High Temperature Epoxy Product Description: EPO TEK® 353ND Black is a a two component, high temperature epoxy designed for semiconductor, hybrid, fiber optic, and medical applicationsAdvantages & Application Notes: EPO T.. |