Chemical Properties | Metric | English | Comments |
---|---|---|---|
Ionic Impurities - K (Potassium) | 15 ppm | 15 ppm | |
Epoxy Technology EPO-TEK® 353ND-T High Temperature Thixotropic Epoxy Product Description: EPO TEK® 353ND-T is a two component, highly thixotropic epoxy with non-flowing properties and high temperature resistance. Advantages & Application Notes: Suitable for fiber op.. |
|||
Ionic Impurities - K (Potassium) | 15 ppm | 15 ppm | |
Epoxy Technology EPO-TEK® H61 Unfilled Epoxy Adhesive Material Description: A single component, high Tg, electrically insulating epoxy adhesive for semiconductor, microelectronic, and opto-electronic packaging applications. It is a liquid version of E.. |