Chemical Properties | Metric | English | Comments |
---|---|---|---|
Ionic Impurities - K (Potassium) | 31 ppm | 31 ppm | |
Epoxy Technology EPO-TEK® E4110 Electrically Conductive, Silver Epoxy Product Description: EPO-TEK® E4110 is an electrically conductive, silver-filled epoxy paste. This two component system is designed for low temperature curing from ambient to 80°C, although other.. |