Chemical Properties Metric English Comments
Ionic Impurities - Fe (Iron) <= 10 ppm
<= 10 ppm
VDPAAPP3
Solvay RHODAPHOSE® VDPA (WET CAKE) Phosphorus derivative
Identification: VINYLIDENE DIPHOSPHONIC ACID, TETRASODIUM SALT.CAS: 33016 – 77 – 2ELINCS: 443 – 520 – 7Solubility: Soluble in waterAvailable in: Asia Pacific, Europe, Latin America and North Ame..