Chemical Properties | Metric | English | Comments |
---|---|---|---|
Carboxyl End Groups | 50 meq/kg | 50 meq/kg | Titration; Internal Method |
Solvay Specialty Polymers Veradel® 3000RP Polyethersulfone (PESU)
(Unverified Data**) Veradel® 3000RP hydroxyl-functionalized polyethersulfones (r-PESU) is an amorphous, high-temperature sulfone polymer featuring reactive end groups to enhance solubility for dissolving or dispersing.. |