Chemical Properties Metric English Comments
Critical Pressure 24.8 bar
18600 torr
3M Novec™ 7000 Engineered Fluid
3M™ Novec™ 7000 Fluid unique properties make it useful as a low temperature, heat transfer fluid for cooling reactors in pharmaceutical & chemical processing. It's also ideal for low temperature a..